Solid-State ^(13)C NMR Investigation of the Oxidative Degradation of Selectively Labeled Polypropylene by Thermal Aging and γ-Irradiation

Abstract

Unstabilized polypropylene (PP) films having selective ^(13)C isotopic labeling were subjected to thermal aging at 50, 80, and 109 °C and to γ-irradiation at 24 and 80 °C. The oxidized films were examined using solid-state ^(13)C nuclear magnetic resonance (NMR) spectroscopy. Dramatic differences were found in the type and distribution of oxidation products originating from the three carbon atom sites within the PP macromolecule (tertiary carbon, secondary carbon, and methyl side group). Most of the oxidation products that formed on the polymer chain originated through chemical reactions at the PP tertiary carbons. Under all of the aging conditions examined, tertiary peroxides (from the PP tertiary site) were the most abundant functional group produced. Also originating from the PP tertiary carbon were significant amounts of tertiary alcohols, together with several more minor products that included "chain-end" methyl ketones. No significant amount of peroxides or alcohols associated with the PP secondary carbon sites was detected. A substantial yield of carboxylate groups was identified (acids, esters, etc.). The majority of these originated from the PP secondary carbon site, from which other minor products also formed, including in-chain ketones. We found no measurable yield of oxidation products originating from reaction at the PP methyl group. Remarkably similar distributions of the major oxidation products were obtained for thermal aging at different temperatures, whereas the product distributions obtained for irradiation at the different temperatures exhibited significant differences. Time-dependent concentration plots have been obtained, which show the amounts of the various oxidation products originating at the different PP sites, as a function of the extent of material oxidation.

Additional Information

© 2005 American Chemical Society. Received 20 December 2004. Published online 12 May 2005. Published in print 1 June 2005. Sandia is a multiprogram laboratory operated by Sandia Corporation, a Lockheed Martin Company, for the United States Department of Energy's National Nuclear Security Administration under Contract DE-AC04-94AL8500. The authors are grateful to Mat Celina for offering valuable comments, to Prof. John Bercaw for cooperation in providing the C(1) labeled PP sample, to Michelle Shedd for DSC measurements, and to Sean Winters and Don Berry for assistance in preparing samples. Impact Analytical (Midland, MI) is acknowledged for acquiring the molecular weight data.

Additional details

Created:
August 19, 2023
Modified:
October 26, 2023